Effects of fly ash and marble waste addition on the thermomechanical properties of an earthenware wall tile composition


ISSN 1121-7588
A.K. Chakrabortya, K.N. Maitib, D.D. Pathakc
aCentral Glass & Ceramic Research Institute, Naroda Centre, Naroda Industrial Estate, India
bEx-Scientist-in-Charge, Central Glass & Ceramic Research Institute, Naroda Centre, Naroda Industrial Estate, India
cDepartment of Applied Chemistry, Indian School of Mines, India

Abstract

The effects of addition of a fly ash-marble waste mixture (2:1), in gradual replacement of sandstone and limestone, on the thermo-mechanical properties of traditional earthenware wall tile composition have been studied. Improvement in mechanical strength of the body was observed by addition of more than 22.5 wt% of the mixture as a substitute for sandstone and limestone at temperature of 1050 °C and above. In this temperature range, water absorption values of the body mixes exhibited a marginal variation (~1%). The improved results encourages the utilization of hazardous waste materials like fly ash and marble waste in the production of value added traditional ceramic product like glazed wall tile.
€ 45,00

ico-info Address
  • Sede legale : via dei Bianchi n.19
  • 47121 - Forlì (FC)
  • email: info@technagroup.it
  • R.E.A. 297724
  • reg. Imp. Forlì-Cesena
  • Capitale sociale: EURO 20.000,00 interamente versato
© Techna Group s.r.l. - Faenza (RA) - Italy - VAT IT03368230409 Daisuke Ecommerce